All tubular metal must be internally and externally drilled to allow drainage of moisture as well as fluids accumulated during pretreatment phase. Any fluid trapped internally during baking stage will boil out, destroying finished paint or possible damage to product. Please call if you have any question on required hole locations. |
|
||||
|
|
|
[